You are here: Products > Anodes - Impressed Current

TELPRO - Mixed Metal Oxide Canisterd Mesh Anodes

TELPRO - Mixed Metal Oxide Canisterd Mesh Anodes

TELPRO MESH STRIP ANODES are manufactured using titanium expanded mesh substrate, which meets ASTM B265 Grade 1 or 2 standards, and TELPRO MMO Coating.

TELPRO MESH STRIP ANODES are 1.25" wide x 48" long and are rated 5 amps for a 20 year design life in calcined petroleum coke. The MESH STRIP ANODE can be packaged in a spiral wound, galvanized steel canister or a fabric sleeve.

TELPRO MIXED METAL OXIDE COATING

TELPRO Mixed Metal Oxide Coating has been designed for use in all cathodic protection applications. TELPRO coating consists of IrO2/Ta2O5 and is suitable for use in soils, carbonaceous backfill, fresh and brackish water, seawater and concrete. Mixed metal oxide coating is generally accepted by the cathodic protection industry to be satisfactory for both chlorine and oxygen evolving electrolytes.

Based on accelerated life testing conducted by an independent laboratory, TELPRO MMO coating has proven to be superior to other mixed metal oxide coatings currently being used. A copy of this test report is available upon request.

Strict quality control procedures are followed throughout the coating process to insure proper coating adhesion and loading. Production of a quality product is fundamental in every step of the manufacturing process.

The operating characteristics for TELPRO MMO coating loadings are shown below:

Environment Maximum Current Density Lifetime
Carbonaceous Backfill 4.6 A/ft2 (50A/m2)

20 years

Calcined Petroleum 9.3 A/ft2 (100A/m2) 20 years
Backfill 9.3 A/ft2 (100A/m2) 20 years
Fresh Water 9.3-27.8 A/ft2 (100-300A/m2) 20 years
Brackish Water 55.8 A/ft2 (600A/m2) 20 years
SKU#:
Quantity: